From: The effect of the different restorations on fracture resistance of root-filled premolars
Groups | Mean (g) ± Standard Deviation | p |
---|---|---|
Group 1 (Positive control) | 1.1645 ± 0.1008 A | 0.860 |
Group 2 (Negative control) | 1.2889 ± 0.1049 A | |
Group 3 (Composite resin) | 1.0600 ± 0.1318 A | |
Group 4 (Fiber+composite resin) | 1.0643 ± 0.2257 A | |
Group 5 (Ceramic Inlay) | 1.2363 ± 0.0985 A |