Skip to main content

Table 4 Mean values of color change of different filling materials after exposure to tea

From: In vitro evaluation of dental color stability using various aesthetic restorative materials after immersion in different drinks

Time-line

Micro-hybrid

Nano-hybrid

Glass-ionomer

∆L

∆a

∆b

∆L

∆a

∆b

∆L

∆a

∆b

Day 7

− 7.28 ± 1.09

8.9 ± 2.68

6.28 ± 3.76

− 6.34 ± 1.02

− 0.76 ± 0.56

5.84 ± 2.82

− 6.84 ± 1.23

1.92 ± 1.92

− 0.18 ± 2.15

Day 30

− 12.16 ± 1.74

11.4 ± 3.82

9.94 ± 4.0

− 9.2 ± 1.2

5.0 ± 3.75

10.78 ± 3.55

− 10.96 ± 4.22

4.48 ± 1.65

− 0.5 ± 1.3