Table 3 Biaxial flexural strength result (mean ± SD) (MPa)

From: Effect of thermocycling on the mechanical properties of permanent composite-based CAD-CAM restorative materials produced by additive and subtractive manufacturing techniques

Material

Non-aging

Aging

CS

296.11 ± 11.56a

278.05 ± 6.11a

VE

173.99 ± 1.99c

173.63 ± 4.77c

VM

173.49 ± 3.47c

153.49 ± 5.37c

SC

232.67 ± 5.94b

215.31 ± 6.39b

FP

234.67 ± 6.14b

230.23 ± 10.35b