Skip to main content

Table 6 Mean values for the push-out bond strength (MPa) by restorative group, root third and their interaction

From: Evaluation of mechanical properties of anatomically customized fiber posts using E-glass short fiber-reinforced composite to restore weakened endodontically treated premolars

a. Restorative Group

Group 1

Group 2

Group 3

Group 4

Group 5

b. Root third

10.13 (2.33) A

7.76 (2.34) B

8.77 (1.99) C

11.95 (1.48) D

13.11 (2.15) E

Cervical

Middle

Apical

  

c. Restorative group X Root third

12.25 (2.37) A

11.00 (1.46) B

7.77 (2.45) C

  

Group 1

Group 2

Group 3

Group 4

Group 5

Cervical

12.20 (0.78) A

9.48 (0.40) B

10.25 (0.79) B

13.59 (0.58) C

15.73 0.64) D

Middle

11.08 (0.80) A

9.21 (0.39) B

9.89 (0.70) B

12.05 0.43) C

12.82 0.64) C

Apical

7.11 (0.52) A

4.60 (0.60) B

6.16 (0.36) C

10.21 0.41) D

10.79 0.46) D

  1. Within each raw, values with similar uppercase superscript letters indicate no statistically significant difference (p > 0.05)