Skip to main content

Table 5 Frequencies of common causes of failures of ceramic restorations according to gender

From: Evaluation of the clinical success of four different types of lithium disilicate ceramic restorations: a retrospective study

Causes of failure

Gender

Total

P value

Male

Female

Fracture

135 (26.84)

173 (34.39)

308 (61.23)

0.3

Debonding

30 (5.96)

39 (7.75)

69 (13.72)

 

Marginal adaptation

31 (6.16)

30 (5.96)

61 (12.13)

 

Color match

4 (0.795)

23 (4.57)

27 (5.37)

 

Endodontic intervention

6 (1.19)

5 (0.99)

11 (2.19)

 

Periodontal disease

3 (0.596)

5 (0.99)

8 (1.59)

 

Secondary caries

5 (0.99)

14 (2.78)

19 (3.78)

 

Total

214 (42.54)

289 (57.46)

503 (100)