Table 1 Sample grouping and preservation conditions

From: In-vitro characterization and evaluation of mesoporous titanium dioxide composite hydroxyapatite and its effectiveness in occluding dentine tubules

Groups

Treatment method

Preservation conditions

Control group

The sample surface was not treated

After being embedded in wax, it was stored at 37 °C for 7 days

Gluma group

Dry the sample, dip it in Gluma desensitizer, and smear the sample surface repeatedly for 10 min

HAP group

Dry the sample, dip it in HAP desensitizer, and smear the sample surface repeatedly for 10 min

TiO2–HAP group

Dry the sample, dip it in TiO2–HAP desensitizer, and smear the sample surface repeatedly for 10 min