From: Comparison of retention and fracture load of endocrowns made from zirconia and zirconium lithium silicate after aging: an in vitro study

Fig. 3

Specimens after retention test; a specimen in Zr group with type 3 failure and remaining cement (arrows) on the tooth structure, b specimen in ZLS group with type 2 failure and no remaining cement on the tooth structure, c specimen in ZLS group with fracture within the tooth (n = 1), d specimen in ZLS group with fracture in the pulp chamber part of restoration (n = 3)