Skip to main content

Table 2 The mean mineral density gain difference between 4 groups

From: Chlorhexidine gluconate enhances the remineralization effect of high viscosity glass ionomer cement on dentin carious lesions in vitro

GROUP

A: Equiaâ„¢ (mgHA/ccm)

B: CHX-Equiaâ„¢ (mgHA/ccm)

C: Ketacâ„¢ (mgHA/ccm)

D: CHX-Ketacâ„¢ (mgHA/ccm)

P

Mean mineral density gain (post-restoration)

88.81 ± 59.857

168.29 ± 100.899

165.54 ± 72.366

183.00 ± 73.096

0.045*

Mean mineral density gain (post-pH cycling)

99.20 ± 77.240

169.21 ± 99.199

166.32 ± 74.182

205.15 ± 91.678

0.065

  1. *Comparison the mean mineral density gain post-restoration of 4 groups, significant difference (P < 0.05)