Skip to main content

Table 2 Mean volume losses and standard deviations of the tested ceramics at each checkpoint in mm3

From: Effect of aqueous environment on wear resistance of dental glass–ceramics

Groups

Chewing cycles (× 104)

10

30

50

LD-wet

1.34 ± 0.07 A

6.38 ± 0.85 A

13.01 ± 0.69 A

LD-dry

0.36 ± 0.07 B

1.37 ± 0.09 B

2.69 ± 0.42 B

LEU-wet

1.62 ± 0.14 A

6.53 ± 0.47 A

11.84 ± 0.94 A

LEU-dry

3.64 ± 0.69 C

15.21 ± 0.81 C

34.47 ± 2.34 C

  1. Means with the same capital letter within one row are not statistically different at p = 0.05 (Tukey test)