Table 1 Materials used in the study

From: Effect of contamination of bulk-fill flowable resin composite with different contaminants during packing on its surface microhardness and compressive strength: in vitro study

 

Manufacturer

Composition

Bulk-fill Flowable resin composite

Nexcomp Flow, Meta Biomed, Korea

Nanohybrid flowable composite 40 nanosized filler: Barium Aluminum borosilicate, Bis-GMA, UDMA, Bis-EMA, TMPTMA (75 weight %, 37 volume %)

Hemostatic agent

Hemo Stop solution, JK Dental Vision Company, Egypt

25% Aluminium chloride solution

Artificial saliva

 

Prepared by mixing of 0.4 g sodium chloride (NaCl), 1.21 g potassium chloride (KCl), 0.78 g sodium dihydrogen dehydrate (NaH2PO4.2H2O), 0.005 g hydrated sodium sulfide (Na2S.9H2O), and 1 g urea CO(NH2)2 in 1000 ml deionized water. The pH of this mixture was modified with 10 N sodium hydroxide until it reached 6.7 on a pH meter [15]

Alcohol

Safwa Company, Egypt

70% Ethyl alcohol

Powdered gloves

SRI Trang Argo-Industry Public Company, LTD, Thailand

Powdered Latex examination gloves