Table 2 Mean value and standard deviations (N) and significance of fracture load test. Different letters indicate that differences were statistically significant (p < 0.05)

From: Effect of abutment design on fracture resistance of resin-matrix ceramic crowns for dental implant restoration: an in vitro study

 

Group

Mean

Standard deviations

Significance

Vita Enamic

1 mm

1545.04

331.74

ab

 

2 mm

1707.09

289.31

a

 

3 mm

1204.96

130.50

b

Lava Ultimate

1 mm

1378.25

232.76

ab

 

2 mm

2222.74

320.36

c

 

3 mm

1383.84

208.54

ab