1) Translucent Prettau Zirconia

Ceramill Zolid HT + White ZrO2

partially stabilized with yttrium and enriched with aluminium

(Ceramill Zolid HT, Amman Girrbach, Germany)

1,909,001

2) Vita Enamic

Polymer infiltrated ceramics VITA ENAMIC blocks

2M2-HT-EM-14

Polymer infiltrated ceramic, SiO2 (58–63), Al2O3 (20–23), Na2O (9–11), K2O (4–6), B2O3 (0.5–2), ZrO2 (< 1), KaO (< 1)

VITA Zahnfabrik, Spitaglasses 3, D-79713 Bad Säckingen, Germany

45,810

3) Nacera Hybrid

Tough, fully polymerized radiopaque composite material with optimized, high-density filler technology (Hybrid A2, Block S)

50% Nano-Glass and 50% Polymer-Matrix

DOCERAM Medical Ceramics GmbH Hesslingsweg 65—67 | D-44309 Dortmund / Germany

100,238

4) High performance

polymer PEKK

PEKKTON ivory milling blank

(98.5/t20mm)

-Polyetherketoneketone

( PEKK) 90%

-Titanium Dioxide (TiO2) 10%

Cendres + Metaux SA, Biel/Bienne, Switzerland

0000347597

5) Nexcomp

Nano-hybrid composite resin

Bis-GMA, UDMA, Bis-EMA

Borosilicate glass

META® BIOMED, Korea

NXC

1,712,112

6) SuperCem,

Self-Etch

Self-Adhesive

Resin Cement

Dual cured dental resin cement, base and catalyst with a dual syringe and mixing tip

Base: Silicon dioxide, Barium glass, BisGMA, Triethyleneglycol Dimethacrylate, Diurethan-dimethacrylate

Catalyst: Silicon dioxide, Barium glass, Tri-ethyleneglycol Dimethacrylate, Diurethan- di methacrylate, Champhorquione

DentKist, Inc, Eli-Dent group S.P.A. KOREA

3,020,004