Skip to main content

Table 3 Fracture resistance (Mean ± standard deviation) of FRRCs

From: Does repeated autoclave sterilization cause changes in the color and fragility of fiberglass reinforced resin crowns?

 

Groups

p value *

Control Group

Group 1

Group 2

Fracture

Resistance

1534.54 ± 285.56

1444.85 ± 156.44

1189.23 ± 196.23

0.055

  1. * p values are based on the one-way Anova test and level of significance was set at p < .05. Fracture resistance values were measured in Newtons (N). Control Group: no sterilization, Group 1: one sterilization, Group 2: four sterilizations with an interval of a day